Hi all

Does anyone know of a published crystal structure for millisite?

It is nominally (Na,K)CaAl6(PO4)4(OH)9·3H2O
Tetragonal, a=7, c=19.07 Å
See http://www.minsocam.org/ammin/AM45/AM45_547.pdf


or maybe anything possibly isostructural/morphous? It's pretty close to
wardite, but has an extra hydroxide and water.

ICDD PDF4+ has nothing, Various searches on COD haven't revealed anything.
I don't have access to ICSD.