I agree with a Ni absorption edge, possibly with a Kβ peak around 38° 2θ.

Tom Gegan
Chemist III

Phone: +1 732 205-5111, Email: tom.ge...@basf.com<mailto:tom.ge...@basf.com>
Postal Address: BASF Corporation, , 25 Middlesex Essex Turnpike, 08830 Iselin, 
United States
[cid:image001.png@01D9DE60.71BF4F10]

From: rietveld_l-requ...@ill.fr <rietveld_l-requ...@ill.fr> On Behalf Of Bish, 
David L
Sent: Sunday, September 3, 2023 7:08 AM
To: Shay Tirosh <stiro...@gmail.com>; Fernando Igoa <fer.igoa.1...@gmail.com>
Cc: Rietveld List (rietveld_l@ill.fr) <rietveld_l@ill.fr>
Subject: [EXT] Re: [External] Re: Step-like basline

Some people who received this message don't often get email from 
b...@indiana.edu<mailto:b...@indiana.edu>. Learn why this is 
important<https://aka.ms/LearnAboutSenderIdentification>
Hello Shay,
I think it is probably related to "tube tails". You can read about this in the 
literature (e.g., on the BGMN web site) and you can model it in some Rietveld 
software such as Topas. You don't normally notice this but it becomes apparent 
with higher-intensity peaks.

Regards,
Dave
________________________________
From: rietveld_l-requ...@ill.fr<mailto:rietveld_l-requ...@ill.fr> 
<rietveld_l-requ...@ill.fr<mailto:rietveld_l-requ...@ill.fr>> on behalf of 
Fernando Igoa <fer.igoa.1...@gmail.com<mailto:fer.igoa.1...@gmail.com>>
Sent: Sunday, September 3, 2023 3:06 AM
To: Shay Tirosh <stiro...@gmail.com<mailto:stiro...@gmail.com>>
Cc: Rietveld List (rietveld_l@ill.fr<mailto:rietveld_l@ill.fr>) 
<rietveld_l@ill.fr<mailto:rietveld_l@ill.fr>>
Subject: [External] Re: Step-like basline

This message was sent from a non-IU address. Please exercise caution when 
clicking links or opening attachments from external sources.

Hey Shay,

Are you using a motorized slit during the measurement? These may open up 
abruptly to compensate for the angular dependence of the footprint and thus 
generate an abrupt increase in the intensity.

Hope it helps :)

On Sun, Sep 3, 2023, 8:50 AM Shay Tirosh 
<stiro...@gmail.com<mailto:stiro...@gmail.com>> wrote:
Dear Rietvelders
I am attaching a zoom-in on a diffraction profile.
My question is what is the origin of the step-like profile next to a very large 
reflection peak?
Is it a sample preparation problem?
Is it part of the baseline?
[cid:image002.png@01D9DE60.71BF4F10]
Thanks
Shay
--









++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list 
<alan.he...@neutronoptics.com<mailto:alan.he...@neutronoptics.com>>
Send commands to <lists...@ill.fr<mailto:lists...@ill.fr>> eg: HELP as the 
subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to