Hello,
At 09:20 PM 3/28/00 +0200, you wrote:
>On the point of view of theory, can the tube-tails and
>Kalpha3 satellite explanations be reconciled ? No tube-tails
>theory in the most recent X-ray powder Diffractometry book
>from Jenkins and Snyder, only Kalpha1, 2, 3, 4, 5, 6.
Don't think so; "Kalpha3" is a component of the emission spectrum of copper
while the "tube tails" appears to be an artifact of poor electron beam
focusing within the X-ray tube.
Jim
James P. Cline [EMAIL PROTECTED]
Ceramics Division Voice (301) 975 5793
National Institute of Standards and Technology FAX (301) 975 5334
100 Bureau Dr. stop 8523
Gaithersburg, MD 20899-8523 USA