Hi,
At 07:31 PM 4/1/00 +0200, you wrote:
> >I'm looking forward for many discussions!
Yep!
>I have some naive questions :
>
>I would like to hear exactly what is on my powder pattern:
> - Kalpha3
> - tube tails
> or both ??
The paper by G. H"olzer et al. (Phys. Rev. A 56 (1997) pp. 4554 ff.) is (at
present) the definitive paper on emission spectra, and they do not discuss
the presence of the "Kalphs3". However, I believe it is referenced
elsewhere (I'll look into it) and, as I have said, it can be readily seen
in the experiment I described previously (anyone who wants a .pdf plot can
email me). I would like to see (or do) the single crystal experiment in
order to definitively characterize the "tube tails". I suspect that the
answer to the Armel's question is both.
>Do these effects would occur at the same angular value ?
Nope; the "Kalpha3" is observed on the low angle side of the profile while
the "tube tails" are observed on both sides.
Regards,
Jim
James P. Cline [EMAIL PROTECTED]
Ceramics Division Voice (301) 975 5793
National Institute of Standards and Technology FAX (301) 975 5334
100 Bureau Dr. stop 8523
Gaithersburg, MD 20899-8523 USA