Dear Prof. Chateigner,

I might need to update my knowledge.
Do we need to consider texture effect for powder samples?


Best Regards!

--

Dr. Xiaodong (Tony) Wang
Senior Research Infrastructure Specialist (XRD)
Central Analytical Research Facility (CARF)   |  Queensland University of 
Technology
Address: Level 6, P Block, Gardens Point campus, 2 George St Brisbane QLD 4000
Tel: +61 7 3138 1904  |   Mob: 0452 571 680
Email:   tony.w...@qut.edu.au   |   Web: www.qut.edu.au/ife/carf





At 2023-11-14 19:58:05, "Daniel Chateigner 20210513" 
<daniel.chateig...@ensicaen.fr> wrote:
>and not textured ?
>
>Le 14/11/2023 à 12:56, Reinhard Kleeberg a écrit :
>> Hi Jim,
>> great news, would be good to have a corundum what can be modelled with 
>> an easier profile shape model.
>> Best regards
>>
>> Reinhard
>>
>> Zitat von "Cline, James P. Dr. (Fed)" <james.cl...@nist.gov>:
>>
>>> Hi all,
>>>
>>> SRM 676a consisted of Baikowski CR1.  This material is of a non-ideal 
>>> crystallite size distribution: quite broad with tales to large 
>>> crystallites.  SRM 676b was custom made for us by Baikowski with a 
>>> more uniform crystallite size distribution in the 200 nm region.  We 
>>> are working on the certification, rather complex, see: 
>>> doi:10.1107/S0108767311014565 .  It seems that modern beamlines don't 
>>> favor the large specimen size needed for our experiments.  We have 
>>> good data from one source, we are looking for some from another as we 
>>> like to see results from more one machine.
>>>
>>> Jim
>>>
>>>
>>> James P. Cline
>>> Materials Measurement Science Division
>>> National Institute of Standards and Technology
>>> 100 Bureau Dr. stop 8370 [ B113 / Bldg 217 ]
>>> Gaithersburg, MD 20899-8523    USA
>>> james.cl...@nist.gov
>>> https://www.nist.gov/people/james-p-cline 
>>>
>>> (301) 975 5793
>>>
>>> -----Original Message-----
>>> From: rietveld_l-requ...@ill.fr <rietveld_l-requ...@ill.fr> On Behalf 
>>> Of Reinhard Kleeberg
>>> Sent: Monday, November 13, 2023 1:51 AM
>>> To: rietveld_l@ill.fr
>>> Subject: Re: NIST-676a
>>>
>>> We are using Baikowski CR1
>>> https://www.baikowski.com/en/serie/cr/ 
>>>
>>> Not certified but maybe identical with SRM676a. Scale factors and 
>>> cell parameters found to be within the errors. Profile shape shows 
>>> similar features (also not an ideal material).
>>> Best regards
>>> Reinhard
>>>
>>>
>>> Zitat von Matthew Rowles <rowle...@gmail.com>:
>>>
>>>> Hi Matej
>>>>
>>>> You can try IMS135 - high purity alumina.
>>>>
>>>> https://imst/
>>>> andards.com.au%2Fproducts%2F&data=05%7C01%7Cjames.cline%40nist.gov%7C2
>>>> d945a33db074232a69808dbe414ca9a%7C2ab5d82fd8fa4797a93e054655c61dec%7C1
>>>> %7C0%7C638354550207433666%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAi
>>>> LCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C3000%7C%7C%7C&sdata=r
>>>> MK%2BzDuAMv2q7U6fCpu38mzuqIrTdCiQfNDPSmB%2BQZk%3D&reserved=0
>>>>
>>>> It was certified against some SRM676a we already had in the lab.
>>>>
>>>>
>>>> Matthew
>>>>
>>>>
>>>>
>>>>
>>>> On Sun, 12 Nov 2023 at 22:42, Matej Dolenec <smu...@siol.net> wrote:
>>>>
>>>>> Dear all,
>>>>>
>>>>> I am trying to buy NIST-676a but unfortunately unsuccessful ... I was
>>>>> trying to find it on NIST, ALDRICH and other sites but the standard
>>>>> is out of stock. Does anybody has any information if this standard
>>>>> will be available soon and where? If not, which standard should I use
>>>>> instead of NIST-676a? I was using this standard for amorphous phase 
>>>>> identification.
>>>>>
>>>>> Regrads, Matej
>>>>>
>>>>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>>>>> Please do NOT attach files to the whole list
>>>>> <alan.he...@neutronoptics.com
>>>>> >
>>>>> Send commands to <lists...@ill.fr> eg: HELP as the subject with no
>>>>> body text The Rietveld_L list archive is on
>>>>> http://www/.
>>>>> mail-archive.com%2Frietveld_l%40ill.fr%2F&data=05%7C01%7Cjames.cline%
>>>>> 40nist.gov%7C2d945a33db074232a69808dbe414ca9a%7C2ab5d82fd8fa4797a93e0
>>>>> 54655c61dec%7C1%7C0%7C638354550207433666%7CUnknown%7CTWFpbGZsb3d8eyJW
>>>>> IjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C3000
>>>>> %7C%7C%7C&sdata=nnVgkFx8mHZ%2Br%2Bng9oJ00Uz9wBy9MYDZ%2F46l%2F3%2BUGg8
>>>>> %3D&reserved=0
>>>>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>>>>>
>>>>>
>>>
>>>
>>> -- 
>>> TU Bergakademie Freiberg
>>> Dr. R. Kleeberg
>>> Mineralogisches Labor
>>> Brennhausgasse 14
>>> D-09596 Freiberg
>>>
>>> Tel. ++49 (0) 3731-39-3244
>>> Fax. ++49 (0) 3731-39-3129
>>
>>
>>
>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
>> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
>> The Rietveld_L list archive is on 
>> http://www.mail-archive.com/rietveld_l@ill.fr/
>> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>>
>-- 
>
>----------------------------------------------------------------------
>Daniel Chateigner
>Professeur Normandie Universite
>http://www.ecole.ensicaen.fr/~chateign/danielc/
>----------------------------------------------------------------------
>Editor: "Combined Analysis", Wiley-ISTE: 
>http://eu.wiley.com/WileyCDA/WileyTitle/productCd-1848211988.html
>Workshops on Combined Analysis: 
>http://www.ecole.ensicaen.fr/~chateign/formation/
>----------------------------------------------------------------------
>Address:
>CRISMAT-ENSICAEN and IUT-Caen,
>Universite de Caen Normandie, campus 2
>6, Bd. M. Juin 14050 Caen, France
>tel: 33 (0)2 31 45 26 11
>daniel.chateig...@ensicaen.fr
>----------------------------------------------------------------------
>Open Databases:
>Material Properties Open Database (MPOD): mpod.cimav.edu.mx
>Crystallography Open Database     (COD): http://www.crystallography.net/cod/
>                   Theoretical     (TCOD): http://www.crystallography.net/tcod/
>                   Predicted       (PCOD): http://www.crystallography.net/pcod/
>Raman Open Database (ROD): solsa.crystallography.net/rod/
>Full-Profile Search-Match (FPSM): cod.iutcaen.unicaen.fr/
>----------------------------------------------------------------------
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to