Hi Matej You can try IMS135 - high purity alumina.
https://imstandards.com.au/products/ It was certified against some SRM676a we already had in the lab. Matthew On Sun, 12 Nov 2023 at 22:42, Matej Dolenec <[email protected]> wrote: > Dear all, > > I am trying to buy NIST-676a but unfortunately unsuccessful ... I was > trying to find it on NIST, ALDRICH and other sites but the standard is > out of stock. Does anybody has any information if this standard will be > available soon and where? If not, which standard should I use instead of > NIST-676a? I was using this standard for amorphous phase identification. > > Regrads, Matej > > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > Please do NOT attach files to the whole list <[email protected] > > > Send commands to <[email protected]> eg: HELP as the subject with no body > text > The Rietveld_L list archive is on > http://www.mail-archive.com/[email protected]/ > ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ > >
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <[email protected]> Send commands to <[email protected]> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++