Dear Armel,

Thanks for this nice quiz!

However, after identifying the following spectral impurities:
 Cu K_beta,
 W L_alpha1,2
 W L_beta1,2,3,4 and
 W L_gamma1,
I am stuck now, leaving bout 1/2 to 1/3 of the tiny extra peaks unexplained.

Some of them look suspiciously like Cu K_alpha1+2 doublets and might thus belong to an impurity phase, or differently oriented crystallites of the main phase, which could lie as dust on the single crystal surface, but I had no luck trying to identify them.

Furthermore, the irregular high angle tailing of the 00l series (maybe stacking faults?) makes peak fitting difficult.

Thus, I give up (at least for now), hoping that you might disclose the solution to the riddle, as far as it is known, for us after a while.

Best wishes,
Frank



On 06.09.2023 10:47, Le Bail Armel wrote:
Hi,

In the same subject.

A special "powder pattern" to play with (try to explain all peaks) :

http://cristal.org/muscovite.pdf <http://cristal.org/muscovite.pdf>

Best

Armel


++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to