Dear Shay,

Do you use CuKalpha radiation or the like?

Try to get the wavelength for the step and the peak at left. I guess they
are the absorption edge of a filter and Kbeta, respectively.

Best

Miguel


El dom, 3 sep. 2023 9:12, Yoji Kobayashi <[email protected]>
escribió:

> Dear Shay,
>
> Does your diffractometer have a Ni foil filter (to cut K-beta radiation)?
> The absorption edge of Ni often results in this “step” near any strong
> diffraction peak; it is quite normal for such arrangements.
>
> Best,
>
> Yoji
>
> ==========================================================
> Yoji Kobayashi, Assoc. Prof.    يوجي كوباياشي
> [email protected]https://imatreac.kaust.edu.sa
> Office: +966 (0)12-808-7232.   Mobile: +966 (0)54-470-1804
>
> Room 4277, Building 3 (Ibn Sina)
> Chemical Science Program, KAUST Catalysis Center
> Division of Physical Science and Engineering
> King Abdullah University of Science and Technology, Saudi Arabia
> ==========================================================
>
> On 3 Sep 2023, at 9:44 AM, Shay Tirosh <[email protected]> wrote:
>
> Dear Rietvelders
> I am attaching a zoom-in on a diffraction profile.
> My question is what is the origin of the step-like profile next to a very
> large reflection peak?
> Is it a sample preparation problem?
> Is it part of the baseline?
> <image.png>
> Thanks
> Shay
> --
>
>
>
>
>
>
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> https://urldefense.com/v3/__http://www.mail-archive.com/[email protected]/__;!!Nmw4Hv0!w-yODRD0lzZ1lVAeDkHJr5sluosziIfM9HlNeLNAeVkQ2Ae6OCEp41_S7BkW0YXUmBPTUVFpKEddVhhq4fuaVV1NBQ$
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++