Dear James Cline:

I am Dr, Gustavo Cifredo and I am working at the Universidad de Cadiz
(Spain) and I am afraid that I am another one that will be very pleased if
you send to us both the attachement and the manuscript, and also
information about the printers of your book.

Thank you very much in advance.

At 12:08 9/11/98 -0500, you wrote:
>Hi all,
>
>At 09:25 AM 11/9/98 -0500, I wrote:
>>Hi,
>>
>----------------------snip------------------------
>>
>>I have developed and written up a strategy addressing the refinement of
>>profile coefficients for Rietveld analysis of conventional X-ray powder
>>data using GSAS.  Its basic premise is the separation of the instrumental
>>terms from the sample related ones and involves the use of SRMs for
>>verification of instrument performance (surprised?).  The manuscript is
>>part of an update to the workshop notes distributed at "The Design,
>>Alignment, Calibration and Performance Characteristics of the Conventional
>>Laboratory Diffractometer" presented at Denver last year by myself and Bob
>>Cheary.  The manuscript will also appear in a book "Industrial Applications
>>of X-ray Diffraction" edited by D. Smith and F. Chung.  I can send the
>>manuscript as a Word97 attachment upon request.  I can also sent out an
>>full updated a hardcopy of the workshop notes in about a month as we (Bob
>>and I) are working on an update at this time.
>>
>
>I've gotten a bunch of requests.  However, there seems to be some
>confusion.  I can only send out the manuscript, entitled "Use of NIST
>Standard Reference Materials for Characterization of Instrument
>Performance", which covers the Rietveld refinement strategy issue as a
>Word97 file.  The workshop notes are (will be) available in hardcopy only.
>If you would like to receive both the manuscript and the workshop notes
>please indicate this clearly in your request; otherwise I will just send
>you the manuscript as a Word97 attachment.
>
>Regards,
>
>Jim
>
>
>James P. Cline                                 [EMAIL PROTECTED]
>Ceramics Division                                      Voice (301) 975 5793
>A256/223                                               FAX (301) 975 5334
>National Institute of Standards and Technology
>Gaithersburg, MD 20899    USA
>
>

Dr. Gustavo A. Cifredo Chacon
Universidad de Cadiz
Departamento de Ciencias de los Materiales e Ingenieria Metalurgica y
Quimica Inorganica
CASEM 11510 Puerto Real, Cadiz, SPAIN
phone: 956 470856

Reply via email to