Gene; One coat brushed directly to inner surface. As long as the VE has =
not
had wax added or Air Dry no sanding needed. I have been watching the PVA
thread and wondered why go to all the trouble when resin/material =
suppliers
all carry Air Dry which is especially made to eliminate the tackiness
problem and is used for the final lay-up for a smooth slick surface that =
is
tack free. It just mixes with the resin after the hardener has been =
added
according to the manufactures proportions and works like a charm and =
doesn't
clog the sandpaper if later modifications or repairs are required.