KR>Discussion on WAF laser parts

2008-10-12 Thread Leigh Plymale
Right on Mark. 4130 is an air hardening alloy, and can get harder than a > file if cooled quickly, and it would be. > > Heat treating is inexpensive, and would be easy for a WAF set, especially in > quantity. During the switch I don't know if you got my response to this post. So here it is agai

KR>Discussion on WAF laser parts

2008-10-12 Thread Mark Langford
Leigh Plymale wrote: > ... With that in mind, Mark L. didn't you have your panel water jet > cut? This should be a very cool process. How 'bout it? Yes, I had my panel waterjet cut. Details are at http://home.hiwaay.net/~langford/kpanel.html . Waterjet cutting is great for aluminum because it d