Try https://onlinelibrary.wiley.com/iucr/doi/10.1107/S2053273323010550

And

https://journals.iucr.org/paper?ae5125

Matthew

On Thu, 20 Mar 2025, 15:47 Luca Lutterotti, <luca.luttero...@unitn.it>
wrote:

> Nope, I checked what I have and I use Xraylib now in Maud but also there
> is only B neutral. Maybe someone can calculate them?
>
> Ciao Luca
>
> <http://www.unitn.it/>
> [image: logo_unitrento_firma.png]
>
>
>
> *Luca Lutterotti*
> Dipartimento di Ingegneria Industriale
> Università di Trento
> <https://www.google.com/maps/search/Trento+via+Sommarive,+9+-+38123+Trento+(Italy?entry=gmail&source=g>
> via Sommarive, 9 - 38123 Trento (Italy
> <https://www.google.com/maps/search/Trento+via+Sommarive,+9+-+38123+Trento+(Italy?entry=gmail&source=g>
> )
> tel. +39 0461 2824-14 (Office), -34 (X-Ray lab)
>
> [image: ico_fb_32x32.png][image: ico_twitter_32x32.png][image:
> ico_insta_32x32.png][image: ico_linkedin_32x32.png][image:
> ico_youtube_32x32.png]
>
>
> Maud: http://maud.radiographema.com <http://maud.radiographema>
>
>
>
> On 19 Mar 2025, at 20:58, Le Bail Armel <le-bail.ar...@orange.fr> wrote:
>
> Hello,
>
> Any parametrized X-ray scattering factor for B3+ somewhere ?
>
> A case with [BF4] tetrahedra.
>
> Thanks !
>
> Armel
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com
> >
> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com
> >
> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to