Hi,

I'm playing with Fullprof again for the first time in many years since I've 
changed employer and lost my access to Topas.

Is it possible to introduce independent peaks (i.e. peaks whose positions are 
not determined by a unit cell) with refinable positions, intensities and shapes 
in Fullprof? I've found this possibility very useful in Topas for dealing with 
features in the datasets that are not of interest and not possible to possible 
to describe with a crystalline phase e.g. diffuse scattering from an amorphous 
component.

I'm aware of the option to include a self-defined background (.bac file) with 
refinable scale, but this is time-consuming workaround.

Best regards,
Magnus

----
Magnus H. Sørby, PhD
Senior Scientist  - Materials Science and Analytical Chemistry
Cenate AS
Norway

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to