Dear Shay,
The last MAUD version is here, please first check if you run the latest:
http://maud.radiographema.com
Examples of configured experiments including layered samples are also
available at:
http://www.ecole.ensicaen.fr/~chateign/formation/
In the meantime, can you send your .par file for checking ?
sincerely
daniel
Le 02/05/2020 à 13:20, Shay Tirosh a écrit :
Dear Rietvelders
Specifically to the MAUD community.
Some features in MAUD are not working properly (in my case).
For example:
1. I wish to model to layers. The upper layer is a film contains a
mixture of three phases. Beneath a layer (film) with a single phase.
However, it seems that modeling using layers does not work.
Specifically editing layers does not allows picking a few phases in a
single layer. And It is impossible to pick different phases in
different layers. MAUD let me define two layers, each contains all
phases (four phases). I tried to "cheat" and fix the volume fraction
flowing my model and it doesn't work. MAUD does not count layer 2 even
if I nullify the thickness of layer 1.
2. I am unable to create multiple samples (add object does not work).
3. The appearance of all curves in the plot are all black. The data
set color and the computed CIF are black. Also, the color of the
corresponding labeled phases are all black with no option to change it.
Please note that problem 3 has been eliminated in case I am running a
similar project on a different computer (identical MAUD version).
1. Can you comment?
2. Any Suggestions?
Thank you from advance
Shay
--
_________________________________________________
Dr. Shay Tirosh
Institute for Nanotechnology & Advanced Materials
Bar Ilan University
Ramat Gan, 52900
Israel
Phone: +972-(0)30-531-7320
Mobile: +972-(0)54-8834533
Email: stiro...@gmail.com <mailto:stiro...@gmail.com>
_________________________________________________
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
--
----------------------------------------------------------------------
Daniel Chateigner
Professeur Normandie Universite
www.ecole.ensicaen.fr/~chateign/danielc/
----------------------------------------------------------------------
Editor: "Combined Analysis", Wiley-ISTE:
http://eu.wiley.com/WileyCDA/WileyTitle/productCd-1848211988.html
Workshops on Combined Analysis: www.ecole.ensicaen.fr/~chateign/formation/
----------------------------------------------------------------------
Address:
CRISMAT-ENSICAEN and IUT-Caen,
Universite de Caen Normandie, campus 2
6, Bd. M. Juin 14050 Caen, France
tel: 33 (0)2 31 45 26 11
daniel.chateig...@ensicaen.fr
----------------------------------------------------------------------
Open Databases:
Material Properties Open Database (MPOD): mpod.cimav.edu.mx
Crystallography Open Database (COD): www.crystallography.net/cod/
Theoretical (TCOD): www.crystallography.net/tcod/
Predicted (PCOD): www.crystallography.net/pcod/
Raman Open Database (ROD): solsa.crystallography.net/rod/
Full-Profile Search-Match (FPSM): cod.iutcaen.unicaen.fr/
----------------------------------------------------------------------
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++