Dear Rietvelders

Specifically to the MAUD community.
Some features in MAUD are not working properly (in my case).
 For example:
1. I wish to model to layers. The upper layer is a film contains a mixture
of three phases. Beneath a layer (film) with a single phase. However, it
seems that modeling using layers does not work. Specifically editing layers
does not allows picking a few phases in a single layer. And It is
impossible to pick different phases in different layers. MAUD let me define
two layers, each contains all phases (four phases). I tried to "cheat" and
fix the volume fraction flowing my model and it doesn't work. MAUD does not
count layer 2 even if I nullify the thickness of layer 1.
2. I am unable to create multiple samples (add object does not work).
3. The appearance of all curves in the plot are all black. The data set
color and the computed CIF are black. Also, the color of the corresponding
labeled phases are all black with no option to change it.

Please note that problem 3 has been eliminated in case I am running a
similar project on a different computer (identical MAUD version).

1. Can you comment?
2. Any Suggestions?

Thank you from advance
Shay



-- 
_________________________________________________

Dr. Shay Tirosh
Institute for Nanotechnology & Advanced Materials
Bar Ilan University
Ramat Gan, 52900
Israel
Phone: +972-(0)30-531-7320
Mobile: +972-(0)54-8834533
Email: [email protected]
_________________________________________________
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

  • [no subject] Shay Tirosh
    • Re: Daniel Chateigner

Reply via email to