Tony, if you bin (add) the raw data you can perform Rietveld refinement as
if you had taken larger steps.
Regards, Alan.

On Thu, 26 Sep 2019 at 05:42, iangie <ian...@126.com> wrote:

> Dear Rietvelder,
>
> I hope you are doing well.
> It is generally acknolwdged that Rietveld refinement should be performed
> on raw data, without any data processing.
> One of our diffractometer/PSD  scans data at its minimal step size (users
> can see that the step size during scan is much smaller than what was set),
> and upon finishing, the measurement software re-bin the counts to the step
> size what users set (so the data also looks smoother, after re-bin).
> My I ask is this re-bined data from the measurement software considered as
> "raw data" or "treated data"? And can we apply Rietveld refinement on this
> data?
>
> Any comments are welcome. :)
>
> --
> *Dr. Xiaodong (Tony) Wang*
> *Research Infrastructure Specialist (XRD)*
> Central Analytical Research Facility (CARF)   |   Institute for Future
> Environments
> Queensland University of Technology
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com
> >
> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>

-- 
______________________________________________
*   Dr Alan Hewat, NeutronOptics, Grenoble, FRANCE *
<alan.he...@neutronoptics.com> +33.476.98.41.68
http://www.NeutronOptics.com/hewat TVA FR 79499450856
______________________________________________
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to