Dear Breogán,

most probably, you have to make alignment of the primary beam cut. If you use focusing mirror, the beam cutter should be there, see the picture here:
https://drive.google.com/file/d/1SLbYfw90cikML_tE19Xp0ZHgBBNtTc9Y/view?usp=sharing


Jan


Dne 2019-06-11 11:17, Cristóbal Verdugo napsal:
Hi Breogan,

Not with Panalytical but with Bruker diffractometer I had the same
problem, we are close to the direct beam. What I did was to cronstruct
a circular slit to cut the direct beam and now I can measure from 2
degrees.
Please, feel free to contact me for help.

Regards,

Cristóbal

—
Dr. Cristóbal Verdugo-Escamilla

cristobal.verd...@csic.es
Phone. 0034 677350122
El 11 jun 2019 11:10 +0200, Breogán Pato Doldán
<breogan.p...@udc.es>, escribió:

Dear Rietvelders,

First of all, I would like to thank you for your help. I joined the
mailing list during the first year of my PhD studies. The Rietveld
mailing list has proved to be a quite useful tool through these
years.

I have just arrived to a new lab and I am the only one with some
XRPD experience.

Several months ago an Empyrean from Panalytical was installed in the
lab. The diffractometer is configured on transmisión. I have had
some problems recording data at low angles (below 5 degrees) ¿Has
anyone had the same problem?

Best regards,

Breogán Pato
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list
<alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no
body text
The Rietveld_L list archive is on
http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to