Dear Davide,
We often purchase 1 micrometer alumina from the following:
Metallurgical Supply Company
713-827-0700
[email protected]
Item # ME-300-C
1.0um Al2O3 powder
~$240/5 pounds
www.metsuco.com
It is sufficient for routine internal-standard quantitative analyses
(and it is quite inexpensive), but you can evaluate it yourself.
Regards,
David
On 1/23/2018 1:05 AM, Davide Levy wrote:
Hi
I would like to buy alumina standard to use for XRD quantitative
analysis. I looked in NIST website and it finished. Sigma-aldrich
sells it but is too expensive.
do you know other suppliers? Or other quantitative analysis standards?
Thanks
*Dr. Davide Levy, Ph.D.*
*
Director of XRD laboratory
Wolfson Applied Materials Research Centre*
*Tel Aviv University,*
*Ramat Aviv, Tel Aviv 69978, Israel*
*Phone: +972-3-6407815 <tel:+972%203-640-7815>*
*Fax: +972-3-6407819 <tel:+972%203-640-7819>*
*http://www3.tau.ac.il/wamrc/ *
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
--
David L. Bish
Department of Earth & Atmospheric Sciences
Indiana University
1001 E. 10th St.
Bloomington, IN 47405
812-855-2039
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++