Hello,
In the photo, the pellet is black and the powder is white. Why is that?
Best
Jon
On December 8, 2017 3:35:20 PM GMT+01:00, "François Goutenoire"
<francois.gouteno...@univ-lemans.fr> wrote:
>Dear Rietveld users,
>
>We observe an unusual asymmetric peak shape on pellet and not when the
>sample has been crushed in powder.
>
>This asymmetry is observed even at high 2theta angle. I would like to
>known if someone has an explanation ?
>
>I have put the data in the link here after
>
>http://perso.univ-lemans.fr/~fgouten/Asymmetry
>
>Best Whishes, François Goutenoire
>
>--
>*********************************************************************************************
>Pr. Francois GOUTENOIRE
>e-mail:francois.gouteno...@univ-lemans.fr
>Tel: 02.43.83.33.54
>FAX: 02.43.83.35.06
>Département des Oxydes et Fluorures
>Institut des Molécules et des Matériaux du Mans
>IMMM - UMR CNRS 6283
>Université du Maine - Avenue Olivier Messiaen
>F-72085 Le Mans Cedex 9
>FRANCE
>*********************************************************************************************
>Formation Rietveld CNRS
>https://cnrsformation.cnrs.fr/stage.php?stage=18098
>Formation SAXS et Réflectivités pour couches minces et matériaux
>nanostructurés.
>https://cnrsformation.cnrs.fr/stage.php?stage=18104
--
Sent from my Android device with K-9 Mail. Please excuse my brevity.
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++