How was the Pellet made? Could be residual stresses on the surface.

Cheers,
Ed

On Fri, Dec 8, 2017 at 9:35 AM, François Goutenoire <
francois.gouteno...@univ-lemans.fr> wrote:

> Dear Rietveld users,
>
> We observe an unusual asymmetric peak shape on pellet and not when the
> sample has been crushed in powder.
>
> This asymmetry is observed even at high 2theta angle. I would like to
> known if someone has an explanation ?
>
> I have put the data in the link here after
>
> http://perso.univ-lemans.fr/~fgouten/Asymmetry
>
> Best Whishes, François Goutenoire
>
> --
> *********************************************************************************************
> Pr. Francois GOUTENOIRE
> e-mail: francois.gouteno...@univ-lemans.fr
> Tel: 02.43.83.33.54
> FAX: 02.43.83.35.06
> Département des Oxydes et Fluorures
> Institut des Molécules et des Matériaux du Mans
> IMMM - UMR CNRS 6283
> Université du Maine - Avenue Olivier Messiaen
> F-72085 Le Mans Cedex 9
> FRANCE
> *********************************************************************************************
> Formation Rietveld CNRShttps://cnrsformation.cnrs.fr/stage.php?stage=18098
> Formation SAXS et Réflectivités pour couches minces et matériaux 
> nanostructurés. https://cnrsformation.cnrs.fr/stage.php?stage=18104
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <alan.he...@neutronoptics.com
> >
> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on http://www.mail-archive.com/
> rietveld_l@ill.fr/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
>


-- 
Dr. Edward A. Laitila
Senior Research Engineer/Scientist II/Adjunct Assistant Professor
Michigan Technological University
Dept. of MSE
Room 628 M&M Building
(906) 369-2041
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to