> About Ba2TeO5, it is said that it is isomorphous with Ba2WO5 and Sr2WO5.
>
> Good work Armel. Yes, sharing of open databases is encouraged :-) But
> please don't attach files.
>
> BTW Armel, Ba2WO5 itself has been determined according to Google:
https://inis.iaea.org/search/searchsinglerecord.aspx?recordsFor=SingleRecord&RN=17058181

You might like to add it to COD :-)