Please excuse my stupid post.. if it's only one layer, you won't see any Bragg 
reflection in the 00l direction.  You need multiple layers for that!  (should I 
withdraw from the group?)

- Kurt

________________________________________
From: Kurt Leinenweber
Sent: Tuesday, November 25, 2014 6:09 PM
To: Nelson Duarte; [email protected]
Subject: RE: XRD graphene

I think graphene is only one layer.... so you should only see 00l reflections.  
It's a 2 dimensional problem.  But I have no actual experience with it (other 
than listening to people talk about it).

- Kurt

________________________________________
From: [email protected] [[email protected]] on behalf of Nelson 
Duarte [[email protected]]
Sent: Tuesday, November 25, 2014 5:34 PM
To: [email protected]
Subject: XRD graphene

Dear rietvelds

We index graphene samples with ICDD card of graphite, correct ?
Wich ICDD card of graphite are usualy used ?

Thanks in advance

Best rergards
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to