I think graphene is only one layer.... so you should only see 00l reflections.
It's a 2 dimensional problem. But I have no actual experience with it (other
than listening to people talk about it).
- Kurt
________________________________________
From: rietveld_l-requ...@ill.fr [rietveld_l-requ...@ill.fr] on behalf of Nelson
Duarte [nelson.dua...@ipn.pt]
Sent: Tuesday, November 25, 2014 5:34 PM
To: rietveld_l@ill.fr
Subject: XRD graphene
Dear rietvelds
We index graphene samples with ICDD card of graphite, correct ?
Wich ICDD card of graphite are usualy used ?
Thanks in advance
Best rergards
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++