Dear Martin,
The main problems of the e.s.u. expressions used in Rietveld programs are the
neglect of correlations between residuals and the loss of interrelations
between particular residuals and particular parameters in terms of their mutual
influence.
Some references on the topic:
J. Appl. Cryst. (1979). 12, 554-563
Acta Cryst. (1982). A38, 264-269
J. Appl. Cryst. (1983). 16, 159-163
J. Appl. Cryst. (1986). 19, 10-18
J. Appl. Cryst. ( 1991). 24, 1-5
J. Appl. Cryst. (1994). 27, 802-844
Best regards,
Leonid
*******************************************************
Leonid A. Solovyov
Institute of Chemistry and Chemical Technology
660036, Akademgorodok 50/24, Krasnoyarsk, Russia
http://sites.google.com/site/solovyovleonid
*******************************************************
________________________________
From: Martin Fisch <m_fi...@bluewin.ch>
To: Leonid Solovyov <l_solov...@yahoo.com>
Sent: Friday, May 2, 2014 2:59 PM
Subject: Re: Phase volume fraction
Hi Leonid
Everyone says that Rietveld s.u.'s are underestimated. Why is this?
Is there any reference to this?
Cheers,
Martin
On 02.05.2014 09:57, Leonid Solovyov wrote:
Dear Apu,
>
>
>If you use the Rietveld-based QPA you may assess the detection limit for a
>phase from the estimated standard uncertainty of its weight (or volume)
>fraction. In this case one should also take into account the fact that the
>Rietveld standard uncertainties of QPA are underestimated about 2-3 times. To
>have more realistic uncertainties you may use DDM:
>http://sites.google.com/site/ddmsuite/
>http://sourceforge.net/p/ddmsuite
>
>
>Best regards,
>Leonid
>
>*******************************************************
>Leonid A. Solovyov
>Institute of Chemistry and Chemical Technology
>660036, Akademgorodok 50/24, Krasnoyarsk, Russia
>http://sites.google.com/site/solovyovleonid
>*******************************************************
>
>
>________________________________
> From: Apu Sarkar <apusar...@gmail.com>
>To: "Leoni, Matteo" <matteo.le...@unitn.it>
>Cc: "rietveld_l@ill.fr" <rietveld_l@ill.fr>
>Sent: Friday, May 2, 2014 3:41 AM
>Subject: Re: Phase volume fraction
>
>
>Yes, I meant detection limit.
>In my sample I have a second phase which dissolves at some
>temperature. I tried to identify the dissolution
temperature using
>XRD. With increasing temperature the peak intensity for
the second
>phase decreased. After certain temperature the peak
disappeared. I
>understand that is not exactly the dissolution
temperature. There is a
>limit of XRD to detect the phase.
>
>Thanks
>Apu
>
>Department of Nuclear Engineering
>NC State University
>Raleigh, USA
>
>
>
>On 5/1/14, Leoni, Matteo <matteo.le...@unitn.it> wrote:
>> I guess you are talking about detection limit only,
not quantification
>> limit, right?
>> The answer largely depends on your material
(scattering power, domain size),
>> tube (sampling volume) and counting time. I have seen
cases where you can
>> clearly see something below 0.1 wt% and cases where
already the percent was
>> off limits.
>> Matteo
>>
>>
-----------------------------------------------------------------
>>
>> Matteo Leoni, PhD
>>
>> DICAM
>> University of Trento
>> via Mesiano, 77
>> 38123 Trento
>> Italy
>>
>> Tel +39 0461 282416 Fax +39 0461 282672
>>
>> e-mail: matteo.le...@unitn.it
>>
----------------------------------------------------------------
>>
>>
>> -----Messaggio originale-----
>> Da: rietveld_l-requ...@ill.fr [mailto:rietveld_l-requ...@ill.fr] Per conto
>> di Apu Sarkar
>> Inviato: giovedì 1 maggio 2014 22.24
>> A: rietveld_l@ill.fr
>> Oggetto: Phase volume fraction
>>
>> Hi,
>> Can any one tell me what is the minimum phase volume
fraction that can be
>> detected by a laboratory X-ray diffractometer. In
there any reference for
>> this.
>>
>> I am using the new Empyrean from PANalytical.
>>
>> Thanks
>> Apu
>>
>> Department of Nuclear Engineering
>> NC State University
>> Raleigh, USA
>>
>
>
>--
>Apu Sarkar
>Postdoctoral Research Scholar
>Department of Nuclear Engineering
>North Carolina State University
>
>Raleigh
>USA
>Mobile: 919-561-9244
>Website: https://sites.google.com/a/ncsu.edu/apu/
>
>++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
>Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
>The Rietveld_L list archive is on
>http://www.mail-archive.com/rietveld_l@ill.fr/
>++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++