Dear All
We have an Anton Paar HTK16 furnace with a Pt strip. I am hoping to calibrate it both thermally and mechanically (height shift) using either alpha alumina or ceria so as to better identify HT phases. Have any of you experience of this, or better suggestions for calibrants? My only serious worry is whether there is any potential for ceria to react with, the Pt strip?
(Perhaps under vacuum?) I'd welcome any advice or suggestions.
                 Yours
                   Rory

************************************
Dr R.M. Wilson,
Experimental Officer & RPS
School of Eng. and Materials,
G27 & G30 X-ray Laboratories,
Francis Bancroft Building
Queen Mary College
University of London
Mile End Road
LONDON E1 4NS
UK
Tel: +44 (0)20 7882 7938
Fax: +44 (0)20 7882 7931
************************************

Reply via email to