In Crysfire, you have to use the import command (IM), not the load command.
Make sure you have used the correct export command in Xfit first I.E "Peaks", 
"Two Theta, All Peak types" in the File Details section.
Regards, Martin
Martin Vickers
Dept. of Chemistry, UCL,
20, Gordon Street
WC1H 0AJ

Subject: Re: Crysfire
Date: Fri, 17 Apr 2009 10:05:22 +0900
From: webrhine.st...@gmail.com
To: leopo...@fq.edu.uy
CC: rietveld_l@ill.fr

I used XFIT to find peak positions and export them. By this way, the peak 
positions DO be in an ascending order of 2-theta. In Crysfire, just load 
command, then the program pops up lines needing sorting. I do not think there 
is any possibilty for mistakes here. Even I reload the data, the same problem. 
Does anyone have idea what is wrong? Thanks.

 