I also believe in R's...
Peter Y. Zavalij wrote:
There are others important criteria of refinement quality implemented
in many software but rarely analyzed or published. These are Rp’ and
Rwp’ calculated with background subtracted from both observed and
calculated data. They are especially important when dealing with high
background cases, e.g. Fe compounds measured using Cu radiation or H
compounds using neutrons.
These R’s are always higher but more realistically showing the quality
of profile fit. I saw neutron refinements with Rwp<10% and completely
wrong phase fitted. Yes! R(Bragg) was near 100% so were Rp’ and Rwp’
but Rp and Rwp were so good…
Peter Zavalij
X-ray Crystallographic Center
University of Maryland
College Park, MD
Office: (301)405-1861
Lab: (301)405-3230
Fax: (301)314-9121
*From:* Whitfield, Pamela [mailto:pamela.whitfi...@nrc-cnrc.gc.ca]
*Sent:* Wednesday, March 04, 2009 8:17 AM
*To:* Jon Wright; olga.smirn...@hw7.ecs.kyoto-u.ac.jp
*Cc:* rietveld_l@ill.fr
*Subject:* RE: cRs
I'll put my tuppence worth in here as there can be another
consideration with high backgrounds.
Normally I wouldn't touch the background, but there are times when a
high background causes an artificially shallow minimum and the
refinement isn't going very far (Rietveld software is usually
minimizing Rwp so starting out with a low Rwp isn't very good).
In this instance making the Rwp worse when the peaks aren't fitting
can help. As a rule, before doing that I'd switch to xye format to
preserve the statistics before doing a linear, across-the-board count
substraction (not attempting to take out any wiggles which will
distort peak shapes, etc - leave that to the background modelling). I
suppose you may introduce some slight distortions into the result but
if the refinement is going nowhere then....
However if you try this approach your final Rwp may end up
significantly worse than other papers in the literature, and there are
occasions when referees can get hung up on residuals when a difference
plot speaks a thousand words (or numbers). I suppose you could always
go back and fit the refined model to the original data to get a
wonderful, if slightly meaningless Rwp for the paper!
Pam
------------------------------------------------------------------------
*From:* Jon Wright [mailto:wri...@esrf.fr]
*Sent:* Wed 04/03/2009 4:00 AM
*To:* olga.smirn...@hw7.ecs.kyoto-u.ac.jp
*Cc:* rietveld_l@ill.fr
*Subject:* Re: cRs
Dear Olga,
As you've noticed, the Rietveld R-factors tell you how well you fit the
pattern, but don't tell you how well you fit the peaks. There is a
correlated intensities R-factor which follows from the methods
outlined in:
J. Appl. Cryst. (2004). 37, 621-628 [ doi:10.1107/S0021889804013184 ]
"On the equivalence of the Rietveld method and the correlated integrated
intensities method in powder diffraction"
W. I. F. David
If I remember well; to get the corresponding Rfactor you just take the
correlated intensities chi^2 for your model and divide by the same
statistic with all I_calc set to zero and perhaps convert to a
percentage. (Hopefully Bill is reading and will correct that if I've
screwed it up).
Fortunately any statistics which rely on peak intensities are open to
abuse by using the wrong cell or space group etc, hence the value of
Rietveld Rfactors and a really high background ;-)
Best,
Jon
Olga Smirnova wrote:
> Dear All,
>
> How is life with conventional R factors when you always have to divide
> by zero background?
> Let's have time. Considering a part of the profile without peaks one
> gets 100% cR.
> I did not give the agreement factor; I would say those cR with all
> non-excluded points is incorrect, but cR for
> points with Bragg contribution is almost the same!
> Do you decrease the Rs by adding the background or do you increase cRs
> by subtracting the background?
>
> OS
>
> PS I did not ask my supervisor before sending such a mail.
>
>
------------------------------------------------------------------------
Internal Virus Database is out-of-date.
Checked by AVG.
Version: 7.5.519 / Virus Database: 269.21.6/1323 - Release Date: 3/10/2008 11:07 AM