I'll put my tuppence worth in here as there can be another consideration with 
high backgrounds.
 
Normally I wouldn't touch the background, but there are times when a high 
background causes an artificially shallow minimum and the refinement isn't 
going very far (Rietveld software is usually minimizing Rwp so starting out 
with a low Rwp isn't very good).  
In this instance making the Rwp worse when the peaks aren't fitting can help.  
As a rule, before doing that I'd switch to xye format to preserve the 
statistics before doing a linear, across-the-board count substraction (not 
attempting to take out any wiggles which will distort peak shapes, etc - leave 
that to the background modelling).  I suppose you may introduce some slight 
distortions into the result but if the refinement is going nowhere then....
 
However if you try this approach your final Rwp may end up significantly worse 
than other papers in the literature, and there are occasions when referees can 
get hung up on residuals when a difference plot speaks a thousand words (or 
numbers).  I suppose you could always go back and fit the refined model to the 
original data to get a wonderful, if slightly meaningless Rwp for the paper!
 
Pam

________________________________

From: Jon Wright [mailto:wri...@esrf.fr]
Sent: Wed 04/03/2009 4:00 AM
To: olga.smirn...@hw7.ecs.kyoto-u.ac.jp
Cc: rietveld_l@ill.fr
Subject: Re: cRs



Dear Olga,

As you've noticed, the Rietveld R-factors tell you how well you fit the
pattern, but don't tell you how well you fit the peaks. There is a
correlated intensities R-factor which follows from the methods outlined in:

J. Appl. Cryst. (2004). 37, 621-628    [ doi:10.1107/S0021889804013184 ]
"On the equivalence of the Rietveld method and the correlated integrated
intensities method in powder diffraction"
W. I. F. David

If I remember well; to get the corresponding Rfactor you just take the
correlated intensities chi^2 for your model and divide by the same
statistic with all I_calc set to zero and perhaps convert to a
percentage. (Hopefully Bill is reading and will correct that if I've
screwed it up).

Fortunately any statistics which rely on peak intensities are open to
abuse by using the wrong cell or space group etc, hence the value of
Rietveld Rfactors and a really high background ;-)

Best,

Jon




Olga Smirnova wrote:
> Dear All,
>
> How is life with conventional R factors when you always have to divide
> by zero background?
> Let's have time. Considering a part of the profile without peaks one
> gets 100% cR.
> I did not give the agreement factor; I would say those cR with all
> non-excluded points is incorrect, but cR for
> points with Bragg contribution is almost the same!
> Do you decrease the Rs by adding the background or do you increase cRs
> by subtracting the background?
>
> OS
>
> PS I did not ask my supervisor before sending such a mail.
>
>



Reply via email to