you can try the COD at:

http://www.crystallography.net/

daniel


> Hi,
>
> does anyone have a freely available structure file for montmorillonite
> (any hydration state)? Also, what is a reasonable Reference Intensity
> Ratio for it? The only ICSD entry has an RIR of over 23, so does
> vermiculite. Why is that so high?
>
> Thank you,
> Maria Chrysochoou
>
>


-- 
Daniel Chateigner
Professeur
CRISMAT-ENSICAEN
Bd. M. Juin
14050 Caen, France
http://www.ecole.ensicaen.fr/~chateign/danielc/