I have always preferred to see data plotted in units of Q (though Q^2 or Q^3 makes sense from a perspective of spreading peaks.) Two-theta made sense only when everyone used CuK alpha (which was never true). Personally, I would be glad to never see another plot of intensity vs. d-space.

On Feb 21, 2007, at 10:29 AM, Von Dreele, Robert B. wrote:

OK, I did play about & display some Q-space (Q=2pi/d) plots in GSAS. It
will be an option in the next release.

It has been an option in LIVEPLOT (EXPGUI) for many years. (Sorry, could not resist.) LIVEPLOT output can be exported WYSIWYG to XMGRACE or as a .csv file.

Brian

********************************************************************
Brian H. Toby, Ph.D.                            office: 630-252-5488
Materials Characterization Group Leader, Advanced Photon Source
9700 S. Cass Ave, Bldg. 433/D003             work cell: 630-327-8426
Argonne National Laboratory         secretary (Marija): 630-252-5453
Argonne, IL 60439-4856         e-mail: brian dot toby at anl dot gov
********************************************************************


Reply via email to