Ron Peterson <[EMAIL PROTECTED]> wrote 19 May 1999:
>see stratlingite:crystal structure ,chemistry ... Eur. J. Mineralogy
>2,841-849(1990)
>amer min 77, 674. (1992)
>
>does anyone know why this isn't in the icsd database?
Or why it isn't in the American Mineral. Soc's own database on:
http://www.geo.arizona.edu/xtal-cgi/test
I can't find it even when I search all entries for vol 77, year 1992,
and it's not in the mineral name index. BTW, this is a nice (free)
database for mineral structures.
I have forwarded this to Bob Downs, hoping that he can tell us.
Alan Hewat, ILL Grenoble, FRANCE <[EMAIL PROTECTED]> tel (33) 4.76.20.72.13
ftp://ftp.ill.fr/pub/dif fax (33) 4.76.48.39.06 http://www.ill.fr/dif/