Figure 1.13 of Book Powder Diffraction Theory and Practice

2014-03-14 Thread Tony Wang
hen plot Figure 1.13, therefore the y- axis in Figure 1.13 missed a factor of "Pi/180". Thanks in advance if anyone could confirm this. Tony Wang Ph.D. of Physics, M.S. of Materials Science, B.S. of Solid-state Electronics Research Assistant | John de Laeder Centre Tel | +6

RE: Figure 1.13 of Book Powder Diffraction Theory and Practice

2014-03-14 Thread Tony Wang
: Tony Wang Cc: rietveld_l@ill.fr Subject: Re: Figure 1.13 of Book Powder Diffraction Theory and Practice Dear Tony, thanks for pointing this out. You are absolutely right. This mistake slipped our proof reading. All the best, Robert. Wang : > Dear Rietvelders, > > > > I m