Dear Rietvelders,

 

I might not be the first to ask this question, but I found the Figure 1.13
of book "Powder Diffraction - Theory and Practice" is problematic.

The equation 40 on the previous page is correct. But the authors seems
wrongly treated "Δθ" as angle not radian when plot Figure 1.13, therefore
the y- axis in Figure 1.13 missed a factor of "Pi/180".

 

Thanks in advance if anyone could confirm this.

 

 

Tony Wang 
Ph.D. of Physics, M.S. of Materials Science, B.S. of Solid-state Electronics

Research Assistant | John de Laeder Centre

Tel | +61 8 9266 7511
Fax | +61 8 9266 4190
Mobile | 0430868691
Email |  <mailto:y.c...@curtin.edu.au> tony.w...@curtin.edu.au 
Web |  <http://curtin.edu.au/> http://www.curtin.edu.au



Curtin University is a trademark of Curtin University of Technology. 
CRICOS Provider Code 00301J (WA), 02637B (NSW)

 

 

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to