Dear LK
Below is the only ICSD structural data available for C4A3S. The
reference is :Saalfeld H, Depmeier W
Kristall und Technik, Vol 7, No. 229
Hope this is the right one. Just out of interest, do you have any
references to this compound's use in Portland
Hongwu,
In fact, reading the instructions provided with GSAS is not much
help, since NT does not use an AUTOEXEC file. The SET commands can be
set up using the system/environment controls in the control panel.
Whilst this allows the windows frontend to GSAS to be called up,
it still can't act
Dear All,
Does anyone know of the existence of structural data for Ushkovite
[ Mg Fe2 (PO4)2 (OH)2 !8H2O . ICDD card no. 35-685 ] - it
is not on the ICSD and a literature search has (so far) been
unsuccessful.
Thanks in advance,
Tom Dyer
Confirmation of reading: your message -
Date:14 Aug 00, 14:27
To: [EMAIL PROTECTED]
Subject: definition of size
Was read at 18:11, 14 Aug 00.
Tom Dyer
Concrete Technology Unit
Dept of Civil Engineering
University of Dundee
Dundee, UK
DD1 4HN
Tel: 01382 348 118
Fax: 01382 3
Probably the best approach is to include a known quantity of an internal
standard in the sample. Sample preparation is very important and you
will have to make sure the standard is carefully weighed and that the
mixiing procedure that is used is efficient. You can then carry out
quantitative Rietve