NIST-676a

2023-11-12 Thread Matej Dolenec
Dear all, I am trying to buy NIST-676a but unfortunately unsuccessful ... I was trying to find it on NIST, ALDRICH and other sites but the standard is out of stock. Does anybody has any information if this standard will be available soon and where? If not, which standard should I use instead o

Re: NIST-676a

2023-11-12 Thread Matthew Rowles
Hi Matej You can try IMS135 - high purity alumina. https://imstandards.com.au/products/ It was certified against some SRM676a we already had in the lab. Matthew On Sun, 12 Nov 2023 at 22:42, Matej Dolenec wrote: > Dear all, > > I am trying to buy NIST-676a but unfortunately unsuccessful

Re: NIST-676a

2023-11-12 Thread SMUDUT
Thank you Matthew, Really appreciate!What about cell parameters and peaks positions? Should I use it from the Nist-676a certificate?MatejPoslano iz Outlook za Android ++ Please do NOT attach files to the whole list Send commands to eg: H

Re: NIST-676a

2023-11-12 Thread Reinhard Kleeberg
We are using Baikowski CR1 https://www.baikowski.com/en/serie/cr/ Not certified but maybe identical with SRM676a. Scale factors and cell parameters found to be within the errors. Profile shape shows similar features (also not an ideal material). Best regards Reinhard Zitat von Matthew Rowle