Re: High temperature standard

2000-03-23 Thread Apurva
At 03:48 PM 3/23/00 +0100, you wrote: >Hello, > >I'm looking for a standard material to use as an internal strandard >(lattice parameter) for High Temperature X-ray diffraction ( range 300-1400K). >I already use silicon, however it can react with other phases. > >Do you have any suggestions? > I

Re: High temperature standard

2000-03-23 Thread Simon Redfern
At 15:48 23/03/00 +0100, you wrote: >I'm looking for a standard material to use as an internal strandard >(lattice parameter) for High Temperature X-ray diffraction ( range 300-1400K). >I already use silicon, however it can react with other phases. Alumina is a possible alternative: we use it rou