At 03:48 PM 3/23/00 +0100, you wrote:
>Hello,
>
>I'm looking for a standard material to use as an internal strandard
>(lattice parameter) for High Temperature X-ray diffraction ( range 300-1400K).
>I already use silicon, however it can react with other phases.
>
>Do you have any suggestions?
>


I have used Gold and Pt. in the past.  They are more inert than Si, but may
still react at the upper part of your range.




************************************************************************
Apurva Mehta                    
SSRL/SLAC                        
PO Box 4349, MS 69                 
Stanford, CA 94309
(650) 926 4791