Hi all,
as announced, there are new PC versions (level 2.3.9) available
on the BGMN server
http://www.bgmn.de
Especially, a new kind of anisotropy was introduced: ANISO4.
It is recommended for strain/stress in the manner
k2=ANISO4
There was an oral presentation of P.W. Stephens entitled
"R
Hi all,
there was a first update of the EFLECH/INDEX beta code up to
level 2.3.9. Level 2.3.7 does not handle Siemens (Bruker) and
Philips data as wanted. This bothers BGMN, too. Therefore,
I will support an update of the BGMN DEMO code in near future.
Cheers,
Joerg Bergmann