2008-10-12 Thread Eduardo Navarrete
Que tal Quique, si es un alivio que alguien hable espanol tambien para poser entender todo detalle, yo estoy construyendo un kr-2, ya tengo hecho los largueros principales y de las alas, la proxima semana empiezo con el fuselaje, y tu en que parte ya estas?? proximamente voy a ponerme mi pagina web

KR> Epoxy T88

2008-10-12 Thread Eduardo Navarrete
thanks james for your answer, what temperature dou you recomend me? here in ecuador the temperature is between 13-19C, --- james escribió: > > Hi Eduardo, I used t-88 on my plane.I had no > problems using it. I also did a number of test > pieces with it, and the WOOD always failed ,leav

KR> Epoxy T88

2008-10-12 Thread larry severson
>what temperature dou you >recomend me? here in ecuador the temperature is >between 13-19C, Optimum temperature for epoxy application is 77 degree F. Air temperature can be lower if the epoxy is heated. Higher temperatures will reduce the working time. Lower temperatures will increase it. Ther

KR> Epoxy T88

2008-10-12 Thread Eduardo Navarrete
Hi, i want to buy a t-88 epoxy in systemthree, what dou you think about this product? did you hear something about systemthree? Salu2 Eduardo Navarrete Quito-Ecuador +593-9-8243079 (cell) +593-2-2344568 (home) +593-2-2906898 (office) "ANDEAN KR2" _

KR> Epoxy T88

2008-10-12 Thread james
Hi Eduardo, I used t-88 on my plane.I had no problems using it. I also did a number of test pieces with it, and the WOOD always failed ,leaving the glue joint intact. It is important that you use it in the recommended temperature range. Jim -- Original Message -