Hi Matteo.

Do you mean the old CHEKCELL
http://ccp14.cryst.bbk.ac.uk/tutorial/lmgp/chekcellb.htm
I am copying this to colleagues who may be able to help you.

Regards Alan
________________________________
Dr Alan Hewat, NeutronOptics
Grenoble, FRANCE (from phone)
[email protected]
+33.476984168 VAT:FR79499450856
http://NeutronOptics.com/hewat
_______________________________


On Thu, 17 Feb 2022, 15:24 Bianchini, Matteo (INT), <
[email protected]> wrote:

> Dear colleagues,
>
> I used in the past the checkcell program.
>
> I have a version more than 10 years old, and cannot find online a more
> recent one (or any site to actually download any version of the program
> from Germany).
>
>
>
> - Does anyone know if a recent version exist, and where to find it?
>
> - Does anyone know an alternative software to use ? Note that this is
> mostly for teaching purposes; I know many programs can browse through all
> space groups and help find the best candidates. But I think checkcell had
> the advantage of being graphical, i.e. one could have the students play
> around with the different space groups and see what extinctions would exist
> and whether they would match the experimental data.
>
>
>
> Thanks in advance
>
>
>
> Kind regards
>
>
>
> Matteo
>
>
>
> ----------------------------------
>
> Prof. Dr. Matteo Bianchini
>
> Lehrstuhlinhaber Anorganische Aktivmaterialien für elektrochemische
> Energiespeicher
>
> Fakultät für Biologie, Chemie und Geowissenschaften
>
> Bayerisches Zentrum für Batterietechnik (BayBatt
> <https://www.baybatt.uni-bayreuth.de/de/index.html>)
>
> Universität Bayreuth
>
> Universitätstraße 30 / Gebäude NWI, Raum 2.0.U1.09
>
> D-95447 Bayreuth
>
> Telefon: +49 (0) 921 / 55-4380
>
> E-Mail: [email protected]
>
> www.bianchini.uni-bayreuth.de
>
> Twitter: @MBianchini87 <https://twitter.com/MBianchini87>
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to