Dear Angel,
the most accurate values you can find will come probably from a complete thermodynamic assessments of the two binary systems done in the frame of the Calphad method.

Here are references for:
Mo-Si: Y. Liu, G. Shao, P. Tsakiropoulos, Thermodynamic reassessment of the Mo±Si and Al±Mo±Si systems, Intermetallics 8 (2000) 953±962 Mo-B: Y. Yang, Y.A. Chang, Thermodynamic modeling of the Mo–Si–B system, Intermetallics 13 (2005) 121–128

There exist perhaps more recent evaluations of the systems. This you can check by studying the citations of these two articles.

Kind regards.
/Jean-Marc


Le 28/02/2019 à 20:02, Angel L. Ortiz a écrit :
Dear colleagues:


Could any of you provide me the standard-state enthalpy (KJ/mol) and entropy 
(Jmol/K) for MoSi2 and MoB2?


Thanks a lot


Regards

Angel
--------------------------------------------------------------
Angel L. Ortiz, PhD
Associate Professor (Reader)
Materials Science and Engineering
Department of Mechanical, Energy and Materials Engineering
University of Extremadura, Badajoz 06006, Spain
(34) 924289600 Ext:86726 (Phone)
(34) 924289601 (Fax)
http://materiales.unex.es/miembros/personal/al-ortiz/index.html
---------------------------------------------------------------

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list<alan.he...@neutronoptics.com>
Send commands to<lists...@ill.fr>  eg: HELP as the subject with no body text
The Rietveld_L list archive is onhttp://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++


--
Jean-Marc Joubert
Chimie Métallurgique des Terres Rares
Institut de Chimie et des Matériaux Paris-Est
UMR 7182 CNRS-Université Paris-Est Créteil
2-8 rue Henri Dunant, 94320 Thiais, France
Laboratory's page:http://www.icmpe.cnrs.fr/spip.php?rubrique70
phone/fax: 33 1 49 78 13 44/12 03
Researcher ID: A-1259-2013, ORCID: 0000-0001-7266-1850
email :joub...@icmpe.cnrs.fr personal page:http://www.icmpe.cnrs.fr/spip.php?article632

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to