Dear Rietveld users,

I am currently testing the Spherical Harmonic Preferential Orientation (SH-OP) correction implemented in the last version of HighScorePlus.

It is working nicely, nevertheless I would like to compare the old March-Dollase correction parameter with the new SH-OP parameters.

Is there a way to calculate the strength of the correction in the case of SH-OP ?.

I have read the archive on the subject, but I did not find a right answer. Or may be a F2 coefficient mentioned by Lucas Lutterotti, but I did not find any formula in order to calculate this value.


I am currently working with two compounds which present high preferential orientation K2SO4 and

NaHCO3 on different diffractometer setting and sample preparation: reflection/transmission, back loading preparation, spread on grease, capillary …..


If any one can help me ? Thank in advance.

François Goutenoire


--
*********************************************************************************************
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*********************************************************************************************
Formation Rietveld CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17082

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to