Dear Alan,
I have a few patterns of samples in 0.3mm Boron-Rich Glass capillaries but
collected in Debye-Scherrer mode.
What does "Capillary Specimen data collected in reflection mode" mean, high
angle peaks only?
Cheers!
--
Yours Sincerely,
Dr. Xiaodong(Tony) Wang
XRD Application Scientist
Bruker Singapore Pte. Ltd.
At 2015-06-15 00:32:03, "Alan Coelho" <alancoe...@bigpond.com> wrote:
Hi all
I'm looking for Capillary Specimen data collected in reflection mode which
shows odd bumps on the peaks. I'm aware that there are supposed to be odd
shaped peaks but I am looking for example data that show it. If anyone has such
data and are willing to part with it then let me know.
cheers
alan
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++