Dear Shay,
Could be that one with a = b ~ c ~ 6.31 A ?
http://www.crystallography.net/4335634.html?cif=4335634
And there is another polymorph :
http://www.crystallography.net/4335634.html?cif=4335638
Both in a recent 2013 paper :
Title of publication : Semiconducting Tin and Lead Iodide Perovskites with
Organic Cations: Phase Transitions, High Mobilities, and Near-Infrared
Photoluminescent Properties
Authors of publication : Constantinos C. Stoumpos; Christos D. Malliakas;
Mercouri G. Kanatzidis
Journal of publication : Inorganic Chemistry
Year of publication : 2013
Journal volume : 52
Pages of publication : 9019 - 9038
Best,
Armel
At 18:18 06/12/2014 +0200, Shay Tirosh wrote:
Dear Reitveldrs
In case someone have, can you please send me the CIF of the cubic Pm3m
phase CH3NH3PbI3.
I was unable to find it on the web.
Thank you from advance
Shay
---
Ce courrier électronique ne contient aucun virus ou logiciel malveillant parce
que la protection avast! Antivirus est active.
http://www.avast.com
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++