Hello, I'm trying to run some old PCR files that I obtained 5 years ago by refining synchrotron data, but I have a problem.
Now I'm working with the February 2008 Fullprof version and when I'm trying to run this old PCR files a "Stop/Warning Box" opens with the warning "Too many reflections or too many points" and the refinement cannot start. I tried to reduce the diffraction pattern by excluding some regions, but nothing changes. How is it possible to overcome this problem? Thank you in advance for your help. Alberto