Dear all, To find the intrumental broadening parameters(u,v,w,a,b) from normal X ray data, we can estimate the FWHM and eta for each peak and then fit them according to the caglioti relations. Is this method also applicable for GIXRD data? Thanking you all,
Prasun Sharma Chowdhury Senior Research Fellow Variable Energy Cyclotron Centre Kolkata 700064, WB, India