Dear Angel,

In general, the LP correction angle is the diffraction angle (2theta) of the 
monochromator crystal. If the primary monochromator is Si(111) then the angle 
is 28.44 for CuK_alpha1.

Best regards,
Leonid

*******************************************************
 Leonid A. Solovyov
 Institute of Chemistry and Chemical Technology
 660049, K. Marx 42, Krasnoyarsk , Russia
 www.icct.ru/eng/content/persons/Sol_LA
 www.geocities.com/l_solovyov
*******************************************************

--- On Thu, 7/23/09, alor...@unex.es <alor...@unex.es> wrote:

> From: alor...@unex.es <alor...@unex.es>
> Subject: RE: LP factor in the Rietveld refinement
> To: "Leonid Solovyov" <l_solov...@yahoo.com>
> Cc: rietveld_l@ill.fr
> Date: Thursday, July 23, 2009, 7:00 AM
> Dear All,
> 
> In this scenario, which should be the number for LP in
> Topas if ones has a
> D8 with a primary monochromator for pure CuKalpha1?
> 
> thanks for the response,
> 
> angel l. ortiz
> 



      