Hello Jorge,
we plan to buy an X-ray microsource plus Image-Plate diffractometer.
Aside from classical single crystal frames you can make
2D-Debye-Scherrer ring frames.
Regards
Julius
Jorge Gonzalez schrieb:
Dear Friends,
I would like to contact with people familiar with x-ray
diffractometers capable of performing both powder and single crystal
measurements. We are planning to buy one and we need some information.
Thank you.
Jorge González González
Escuela de Ciencias Químicas
Universidad de Colima, Colima, México.
TLF: (0052) 312 135 6426
Fax: (0052) 312 315 6585
------------------------------------------------------------------------
Tecnología, moda, motor, viajes,…suscríbete a nuestros boletines para
estar a la última MSN Newsletters
<http://newsletters.msn.com/hm/maintenanceeses.asp?L=ES&C=ES&P=WCMaintenance&Brand=WL&RU=http%3a%2f%2fmail.live.com>
begin:vcard
fn:Dr. Julius Schneider
n:Schneider;Dr. Julius
org;quoted-printable:Earth- and Environmental Sciences, Crystallography Section;Ludwig-Maximilians-Universit=C3=A4t M=C3=BCnchen, Germany
adr;quoted-printable;quoted-printable:Theresienstrasse 41;;Ludwig-Maximilians-Universit=C3=A4t M=C3=BCnchen;M=C3=BCnchen;Bayern;D - 80333;Germany
email;internet:[EMAIL PROTECTED]
tel;work:+49 - 89 - 2180.4354
tel;fax:+49 - 89 - 2180.4334
version:2.1
end:vcard