Thank you very much, Prof. Stephens, my mailing address is bellow.

Congwu Cui
***************************************************************** 
Department of Physiology and Biomedical Engineering 
Alfred 2-404, Mayo Clinic College of Medicine 
200 First Street SW 
Rochester MN 55905 

phone: 507-255-8496 
e-mail: [EMAIL PROTECTED] 
***************************************************************** 




Quoting [EMAIL PROTECTED]:

> I'll mail you some fine Si powder if you send me your address.
> 
> My best guess is that you have a relatively big lump of Si in your
> sample 
> that happens to be lined up to make a bright spot from the bremstrahlung
> 
> part of the spectrum.  It happens to meet some Si Bragg reflection 
> condition for some wavelength in the brems. spectrum.
> 
> ^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~
> Peter W. Stephens