Dear Joy, 

The most of profile analysis softwares are able to calculate integrated 
intensities of diffraction peaks but each one operates differently. 
Personally I use EVA and TOPAS P (solded by BRUKER)and is very easy to find 
them. 

Maria Fabra Puchol
Microanalysies Engineer

Saint-Gobain CREE
550, Avenue Alphonse Jauffret
84306 Cavaillon Cedex-France
[EMAIL PROTECTED] 
telf: +33 (0)4 32 50 09 36
fax: +33 (0)4 32 50 08 51


-----Message d'origine-----
De : mukherjee joy [mailto:[EMAIL PROTECTED] 
Envoyé : vendredi 25 août 2006 15:20
À : [email protected]
Objet : integrated intensity

Dear all
may anyone write me in elaborate the steps for finding out the integrated 
intensity for the diffraction peaks due to the different hkl planes for a 
crystalline material. what are the useful softwares available for this.
warm wishes,
j. mukherjee
FSD, Central Fuel Research India